Congratulations! MER Group Hits New Highs in Lime Kiln Technical Capabilities

Jul 24, 2026

Leave a message

The 800 TPD double-shaft vertical kiln EPC turnkey project invested by Gansu Haixin and executed by MER Group has reached a stable daily production of 920 metric tons. Key indicators include underburning rate <5% and kiln pressure 20kPa. Further capacity expansion to 1000 tons per day is in progress.